RoughInSizing calculators for the trades

Spray foam calculator

Enter the area and the thickness. You get board feet, the real kit count, the R-value from the published test reports rather than thickness × R-per-inch, and a check against the 2021 IECC for your climate zone.

R-values from ICC-ES ESR-5252 and ESR-5254Kit yields from the manufacturers' data sheets2021 IECC Table R402.1.3

Inputs

Area
sq ft
Open cell is cheaper per board foot; closed cell is about twice the R per inch.
Sets the depth the foam has to fit inside.
Thickness
Which line of the code table this has to meet.

Buying (optional)

Leave on none if a contractor is spraying it.
$
Your own quote. Leave at 0 to skip.

Result

Board feet needed
—

R-value by thickness, as the reports print it

These are the tested thermal-resistance tables from two evaluation reports by the same manufacturer, so the open-cell and closed-cell columns are directly comparable: ICC-ES ESR-5254 (Accufoam OC, 0.5 pcf) and ICC-ES ESR-5252 (Accufoam CC-HFO, 2.1 pcf). Both are measured at a 75°F mean temperature, and both round values above 10 to a whole number.

The greyed columns are what you get by multiplying thickness by the 1-inch figure, which is how most spray foam calculators work it out. For open cell the two agree. For closed cell they do not, and the gap grows with thickness — the last column is how much the multiplication overstates the real tested number.

ThicknessOpen cellClosed cellClosed cell
overstated by
Tested× per inchTested× per inch
1 in3.73.77.57.5—
2 in7.37.41415+1
3 in1111.12122.5+1.5
3.5 in1313.02426.3+2.3
4 in1414.82730+3
5 in1818.53437.5+3.5
6 in2222.24145+4
7 in2525.94852.5+4.5
8 in2929.65560+5
9 in3233.36267.5+5.5
10 in36376975+6
11 in4040.77582.5+7.5
12 in4344.48290+8

What a filled cavity actually gets you

Foam sprayed flush to the framing, at the real depth of the lumber. Values marked † fall between two printed rows of the report and are interpolated; the rest are printed figures.

FramingDepthOpen cellClosed cell
2x4 stud wall3.5 in1324
2x6 stud wall5.5 in2037.5†
2x8 joist or rafter7.25 in26†50
2x10 joist or rafter9.25 in33†63.8†
2x12 joist or rafter11.25 in40.8†76.8†

Kit yields: the number on the box is not the number you get

Two-component kits are sold by theoretical yield. Convenience Products says so in its own technical data: “Theoretical yield is used as an industry standard to represent the size of two-component foam kits.” Tiger Foam goes further and prints the gap — the kit it calls a 600 has a theoretical yield of 516 board feet — then tells you to “reduce this theoretical yield by 10-12%”.

KitTypeNameTheoreticalAfter the derate
Tiger Foam TF200SRClosed cell200162.5143–146
Tiger Foam TF600SRClosed cell600516454–464
Convenience Products Foam Kit 300Open cell300300264–270
Convenience Products Foam Kit 1000Open cell10001000880–900
Convenience Products CP1200FROpen cell120012001056–1080

2021 IECC minimum R-values by climate zone

Table R402.1.3, as tabulated by PNNL’s Building America Solution Center. “ci” is continuous insulation — a layer outside the framing, which cavity foam is not. The wall column matters most: where it reads 30 or 20+5ci, the all-cavity option is R-30, and that is the number foam between the studs has to reach on its own.

Climate zoneCeilingWood frame wallFloorBasement wallCrawl wall
Zone 13013 or 0+10ci13none requirednone required
Zone 24913 or 0+10ci13none requirednone required
Zone 34920 or 13+5ci or 0+15195ci or 13f5ci or 13f
Zone 4 except Marine6030 or 20+5ci or 13+10ci or 0+20ci1910ci or 1310ci or 13
Zone 5 and Marine 46030 or 20+5ci or 13+10ci or 0+20ci3015ci or 19 or 13+5ci15ci or 19 or 13+5ci
Zone 66030 or 20+5ci or 13+10ci or 0+20ci3015ci or 19 or 13+5ci15ci or 19 or 13+5ci
Zone 7 and 86030 or 20+5ci or 13+10ci or 0+20ci3815ci or 19 or 13+5ci15ci or 19 or 13+5ci
The kit arithmetic that catches people out. Say you need 1,000 board feet and you are buying the kit called 600. Divide by the name and you buy 2. Divide by the theoretical yield of 516 and you still buy 2. Apply the manufacturer’s own 10–12% derate and a kit really lays down about 454 board feet, so you need 3. Buying by the number on the box leaves you a kit short with the job half sprayed and a tank you cannot pause.

Board feet, and why the unit matters

Spray foam is sold by the board foot: one square foot at one inch thick. Area × thickness, and that is the whole conversion. 1,000 sq ft at 3 in is 3,000 board feet whether it is a wall, a roofline or a crawl space.

Because thickness is a straight multiplier on cost, the open-cell-versus-closed-cell decision is mostly a question of how many inches you need to reach the R-value, not of the price per board foot. An attic roofline of 1,500 sq ft that has to reach R-60 in climate zone 5 needs about 16.7 in of open cell (25,000 board feet) or about 8.7 in of closed cell (13,071 board feet). Closed cell is dearer per board foot, but that is 48% fewer board feet, and it is the only one of the two that fits.

The 2x4 wall problem

This is the answer most spray foam pages will not give you. Fill a 2x4 cavity with open-cell foam and you get R-13. Fill it with closed cell and you get R-24. In climate zone 5 the all-cavity path in the IECC table is R-30. Neither one passes, and no amount of foam will fix it, because 3.5 in is all the room there is. A 2x4 wall in zone 5 reaches code through one of the continuous-insulation paths — 30 or 20+5ci or 13+10ci or 0+20ci — which means exterior foam board, not more spray foam in the bay.

Move to 2x6 and the picture changes. Open cell fills 5.5 in for R-20, which still misses. Closed cell reaches R-37.5, which clears R-30 on the cavity-only path. That single fact — 2x6 and closed cell, or add continuous insulation — decides most wall assemblies in the cold zones.

Why the per-inch number overstates thick foam

Closed-cell foam does not deliver the same R for every inch. ESR-5252 prints R-7.5 at one inch and R-82 at twelve. Take the first inch off both and the 11 inches in between are worth about R-6.77 each. The first inch is the best one, and every inch after it is worth about 10% less. Multiply 12 by 7.5 and you get R-90, which is 8 points (9%) more than the report allows — the kind of error that passes a plan check and fails an inspection.

Open cell behaves differently, and it is worth being precise about why. Its first inch is R-3.7 and the inches after it are worth about R-3.61, which is close enough to call flat. Most of the gap you see in the table above is not the foam at all — it is the report rounding every value over 10 down to a whole number. At the full 18 in the shortcut still runs 1.6 points high, about 2%, so it is small rather than absent. The tables above use the published figures either way.

Two code requirements that are easy to miss. Foam plastic has to be separated from the living space by an approved thermal barrier, which the IRC defines as ½ in gypsum wallboard or an approved equivalent (R316.4). Left exposed in a finished space, the foam does not comply no matter how well it insulates. In an attic or crawl space entered only to service utilities, a lighter ignition barrier is allowed instead (R316.5.3 and R316.5.4), or the foam can be covered with a coating that has been tested and listed for the purpose in its evaluation report.

Ignition barrier materials the IRC lists

MaterialMinimum thickness
Mineral fiber insulation1-1/2 in
Wood structural panel1/4 in
Particleboard3/8 in
Hardboard1/4 in
Gypsum board3/8 in
Corrosion-resistant steel0.016 in

Open cell or closed cell

Open cell is about 0.5 lb/ft³, R-3.7 per inch, and vapour permeable — around 10 perms at 5 in, so it is not a vapour retarder and the assembly has to be able to dry. It is the cheaper option per board foot and the usual choice for an attic roofline where there is depth to spare.

Closed cell is about 2.1 lb/ft³, R-7.5 for the first inch, and under 1 perm at 2 in, which makes it a vapour retarder in its own right. It adds structural stiffness and it is the one to use where depth is tight, where the foam has to double as the vapour control layer, or anywhere it may get wet — rim joists, crawl space walls, the underside of a floor over a vented space.

That last one has a trap in it. A crawl space wall in zone 5 wants R-15 of continuous insulation. Two inches of closed cell is R-14, which misses it by one point. You need 2.17 in, so the sprayer has to be told 2¼, not 2.

What this does not do

  • It does not price the job. Installed spray foam is quoted per board foot and the rate swings with region, access and crew, so the price field takes your own quote rather than inventing a number.
  • It does not design a vapour control strategy. Whether an assembly can dry, and in which direction, depends on the climate, the cladding and the interior finish. That is an assembly question, not a thickness question.
  • It does not check whether an unvented attic is permitted. IRC R806.5 sets conditions on air-impermeable insulation applied to the underside of roof sheathing, including condensation control in colder zones.
  • It does not cover the thickness limits in a specific product’s evaluation report. Those reports cap the lift thickness per pass and the total thickness where no prescriptive thermal barrier is used.

Questions

How many board feet is a 2x4 wall?

A board foot is one square foot at one inch thick, so a 2x4 cavity filled flush is 3.5 board feet for every square foot of wall. A 1,000 sq ft wall filled with foam is 3,500 board feet. The framing takes up roughly 15% of a wall's face, so an estimate based on gross wall area has a little slack in it, which is about right once you allow for trimming overspray.

Does spray foam meet code in a 2x4 wall?

In climate zones 1, 2 and 3, yes with closed cell: 3.5 in gives R-24 against a requirement of R-13 or R-20. In zones 4 through 8 the all-cavity requirement is R-30, and a 3.5 in cavity tops out at R-24 with closed cell and R-13 with open cell, so neither passes. Those zones need one of the continuous-insulation paths instead, which means rigid foam outside the sheathing.

How much does one kit of spray foam cover?

Less than the name suggests. The figure in a kit's name is a theoretical yield at one inch, and manufacturers tell you to reduce it. Tiger Foam's own data sheet puts the TF600SR at 516 theoretical board feet and says to take 10 to 12% off that, so about 454 to 464 board feet in practice. Cold tanks make it worse; the chemicals want to be 70 to 90 degrees before you pull the trigger.

Is closed cell twice as good as open cell?

Per inch, roughly: R-7.5 against R-3.7 for the first inch. Per board foot it is closer than that, because closed cell costs more and its R per inch drops as the lift gets thicker. Where there is depth to spare, such as an attic roofline, open cell often reaches the same R-value for less money. Where depth is tight, closed cell is the only one that fits.

Do I need a thermal barrier over spray foam?

Against a living space, yes. IRC R316.4 requires foam plastic to be separated from the interior by an approved thermal barrier, with half-inch gypsum wallboard as the prescriptive option. In an attic or crawl space that is entered only to service utilities, R316.5.3 and R316.5.4 allow a lighter ignition barrier instead, and some products are listed for a tested coating in place of either.

Why is my R-value lower than thickness times R-per-inch?

Because R per inch is not constant for closed cell. The evaluation report for the product used here prints R-7.5 at one inch but R-82 at twelve, which is R-6.83 per inch. The reports also round every value above 10 down to a whole number. Multiplying by the one-inch figure overstates a 12 in application by 8 points, so use the published table when a number has to survive an inspection.

Sources

Codes are adopted and amended locally. Check the edition in force where you work.

More Interiors calculators